Polyphenylene ether (PPE) is an amorphous thermoplastic characterized by high heat resistance, excellent dimensional stability, and low moisture absorption. The material also offers good chemical resistance and electrical insulation properties. PPE is almost exclusively offered as a blend with other plastics, often polystyrene, as pure PPE oxidizes very easily at temperatures above 100°C.
| 製品コード | 製品名 | 形状 | 形状 | 色 | 製品サイズ | 長さ | 幅 | 厚み | 高さ | ||
|---|---|---|---|---|---|---|---|---|---|---|---|
| 在庫なし(MOQあり) | 700145 | SustaPPE black extruded | 丸棒 | 丸棒 | black | Ø 36 x 3000 mm | 3,000 mm | 36 mm | |||
| 在庫なし(MOQあり) | 745214 | SustaPPE black extruded | 丸棒 | 丸棒 | black | Ø 40 x 3000 mm | 3,000 mm | 40 mm |
| 試験法 | 単位 | 数値 | |
|---|---|---|---|
| 密度 | DIN EN ISO 1183-1 | g / cm3 | 1,10 |
| 吸水率 | DIN EN ISO 62 | % | 0,1 |
| 燃焼性 (厚み 3 mm / 6 mm) | UL 94 | HB / HB |
| 試験法 | 単位 | 数値 | |
|---|---|---|---|
| 引張降伏応力 | DIN EN ISO 527 | MPa | 50 |
| 引張破壊呼び歪 | DIN EN ISO 527 | % | 10 |
| 引張弾性率 | DIN EN ISO 527 | MPa | 2400 |
| ノッチ付き衝撃耐性 | DIN EN ISO 179 | kJ / m2 | 11 |
| ショア硬度 | DIN EN ISO 868 | scale D | 82 |
| 試験法 | 単位 | 数値 | |
|---|---|---|---|
| 融点 | ISO 11357-3 | °C | - |
| ガラス転移温度 | ISO 11357-3 | °C | 150 |
| 熱伝導率 | DIN 52612-1 | W / (m * K) | 0,23 |
| 熱容量 | DIN 52612 | kJ / (kg * K) | 1,20 |
| 線膨張係数 | DIN 53752 | 10-6 / K | 80 |
| 使用温度(長期) | 平均値 | °C | -40 … 100 |
| 使用温度(短期、最大) | 平均値 | °C | 110 |
| 荷重たわみ温度 | DIN EN ISO 75, Verf. A, HDT | °C | 100 |
| 試験法 | 単位 | 数値 | |
|---|---|---|---|
| 誘電率 | IEC 60250 | 2,8 | |
| 誘電正接 (50 Hz) | IEC 60250 | 0,008 | |
| 体積固有抵抗 | DIN EN 62631-3-1 | Ω * cm | 1015 |
| 表面固有抵抗 | DIN EN 62631-3-2 | Ω | 1015 |
| 比較トラッキング指数 | IEC 60112 | 450 | |
| 絶縁破壊電圧 | IEC 60243 | kV / mm | 30 |