試験法 | 単位 | 数値 | |
---|---|---|---|
Standard Color | Black | ||
耐薬品性 | Very Good |
試験法 | 単位 | 数値 | |
---|---|---|---|
曲げ強度 | ASTM D 790 | psi | 55,000 |
IZOD Impact Strength (notched) | ASTM D 256 | ft. lb./in. | 15 |
試験法 | 単位 | 数値 | |
---|---|---|---|
熱伝導率 | ASTM C 177 | 2.0 | |
Coefficient of Thermal Expansion, parallel | ASTM D 696 | 10-6 K-1 | 7.1 |
Coefficient of Thermal Expansion, perpindicular | ASTM D 696 | 10-6 K-1 | 20.5 |
Glass Transition Temperature, Tg | ASTM E 1356 | °F | 345 |
Thermal Decomposition Temperature @1% loss | ASTM E 1641 | °F | 440 |
Thermal Decomposition Temperature @5% loss | ASTM E 1641 | °F | 550 |
Thermal Decomposition Temperature @10% loss | ASTM E 1641 | °F | 622 |
表面最高使用温度 | °F | 572 | |
Solder Heat Resistance 10 min. @500°F | Pass |
試験法 | 単位 | 数値 | |
---|---|---|---|
UL Subject 94 | UL 94 | HB |
試験法 | 単位 | 数値 | |
---|---|---|---|
Water Absorption | ASTM D 570 | % by wt. | <0.2 |
比重 | ASTM D 792 | 1.84 | |
Barcol Hardness | ASTM D 2583 | 90 |
試験法 | 単位 | 数値 | |
---|---|---|---|
Surface Resistivity | ASTM D 4496 | Ω/square | 105 - 109 |
Volume Resistivity | ASTM D 4496 | Ω/square | 105 - 109 |
ESD Safe | Yes |