Polystone® M is an ultra-high molecular weight polyethylene (PE-UHMW/PE 1000) used to solve friction, wear and material flow problems in many industries. The material is characterized by excellent sliding properties, extreme wear resistance, high impact strength and very good resistance to chemicals and has established itself in technical applications. The material is available in various colors.
Test Method | Unit | Guideline Value | |
---|---|---|---|
Hustota | DIN EN ISO 1183-1 | g / cm3 | >0,93 |
Absorpce vody | DIN EN ISO 62 | % | 0,01 |
Hořlavost (tloušťka 3 mm / 6 mm) | UL 94 | HB | |
Molecular weight | - | 106 g/mol | ∼ 9 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Prodloužení při přetržení | DIN EN ISO 527 | % | >50 |
Modul pružnosti v tahu | DIN EN ISO 527 | MPa | >650 |
Vrubová houževnatost | DIN EN ISO 11542 | kJ / m2 | >100 |
Tvrdost Shore | DIN EN ISO 868 | scale D | >63 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Teplota tání | ISO 11357-3 | °C | 130 ... 135 |
Tepelná vodivost | DIN 52612-1 | W / (m * K) | 0,40 |
Thermal capacity | DIN 52612 | kJ / (kg * K) | 1,90 |
Koeficient lineární teplotní roztažnosti | DIN 53752 | 10-6 / K | 150 ... 230 |
Provozní teplota dlouhodobá | Průměr | °C | -250 … 80 |
Provozní teplota krátkodobá (max.) | Průměr | °C | 130 |
Teplota měknutí dle Vicata | DIN EN ISO 306, Vicat B | °C | 80 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Relativní permitivita | IEC 60250 | 2,3 | |
Dielektrický disipační faktor (106 Hz) | IEC 60250 | 0,0001 | |
Objemový odpor | DIN EN 62631-3-1 | Ω * cm | >1014 |
Surface resistivity | DIN EN 62631-3-2 | Ω | >1014 |
Comparative tracking index | IEC 60112 | 600 | |
Dielectric strength | IEC 60243 | kV / mm | >40 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Hustota | DIN EN ISO 1183-1 | g / cm3 | >0,93 |
Absorpce vody | DIN EN ISO 62 | % | 0,01 |
Hořlavost (tloušťka 3 mm / 6 mm) | UL 94 | HB | |
Molecular weight | - | 106 g/mol | ∼ 9 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Prodloužení při přetržení | DIN EN ISO 527 | % | >50 |
Modul pružnosti v tahu | DIN EN ISO 527 | MPa | >650 |
Vrubová houževnatost | DIN EN ISO 11542 | kJ / m2 | >100 |
Tvrdost Shore | DIN EN ISO 868 | scale D | >63 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Teplota tání | ISO 11357-3 | °C | 130 ... 135 |
Tepelná vodivost | DIN 52612-1 | W / (m * K) | 0,40 |
Thermal capacity | DIN 52612 | kJ / (kg * K) | 1,90 |
Koeficient lineární teplotní roztažnosti | DIN 53752 | 10-6 / K | 150 ... 230 |
Provozní teplota dlouhodobá | Průměr | °C | -250 … 80 |
Provozní teplota krátkodobá (max.) | Průměr | °C | 130 |
Teplota měknutí dle Vicata | DIN EN ISO 306, Vicat B | °C | 80 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Relativní permitivita | IEC 60250 | 2,3 | |
Dielektrický disipační faktor (106 Hz) | IEC 60250 | 0,0001 | |
Objemový odpor | DIN EN 62631-3-1 | Ω * cm | >1014 |
Surface resistivity | DIN EN 62631-3-2 | Ω | >1014 |
Comparative tracking index | IEC 60112 | 600 | |
Dielectric strength | IEC 60243 | kV / mm | >40 |