Sustarin® H, often known on the market as ‘Delrin’, the brand name of the raw material manufacturer, has a slightly higher density, stiffness and strength compared to Sustarin® C. The chemical resistance, in particular the hydrolysis resistance of Sustarin® H is significantly worse than that of the copolymer. Sustarin® C (FG) should therefore be used in preference, especially in the food industry, where hot water is frequently used for cleaning. The homopolymer has an advantage in applications with high mechanical loads.
Test Method | Unit | Guideline Value | |
---|---|---|---|
Hustota | DIN EN ISO 1183-1 | g / cm3 | 1,42 |
Absorpce vody | DIN EN ISO 62 | % | 0,2 |
Hořlavost (tloušťka 3 mm / 6 mm) | UL 94 | HB / HB |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Mez kluzu | DIN EN ISO 527 | MPa | 75 |
Prodloužení při přetržení | DIN EN ISO 527 | % | 30 |
Modul pružnosti v tahu | DIN EN ISO 527 | MPa | 3200 |
Vrubová houževnatost | DIN EN ISO 179 | kJ / m2 | 10 |
Tvrdost Shore | DIN EN ISO 868 | scale D | 83 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Teplota tání | ISO 11357-3 | °C | 175 |
Tepelná vodivost | DIN 52612-1 | W / (m * K) | 0,31 |
Tepelná kapacita | DIN 52612 | kJ / (kg * K) | 1,50 |
Koeficient lineární teplotní roztažnosti | DIN 53752 | 10-6 / K | 100 |
Provozní teplota dlouhodobá | Průměr | °C | -50 … 90 |
Provozní teplota krátkodobá (max.) | Průměr | °C | 150 |
Teplota tepelné deformace | DIN EN ISO 75, Verf. A, HDT | °C | 110 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Relativní permitivita | IEC 60250 | 3,8 | |
Dielektrický disipační faktor (50 Hz) | IEC 60250 | 0,002 | |
Objemový odpor | DIN EN 62631-3-1 | Ω * cm | 1015 |
Povrchový odpor | DIN EN 62631-3-2 | Ω | 1015 |
Srovnávací sledovací index | IEC 60112 | 600 | |
Dielektrická pevnost | IEC 60243 | kV / mm | 25 |