Characteristics

  • Electrically conductive
  • Good UV resistance
  • Good resistance against many solvents

Technical Specifications Sustarin® C ESD 60 - ASTM

Test MethodUnitGuideline Value
DensityASTM D792g / cm31.44
Water AbsorptionASTM D570%1.0-2.0
Water Absorption 24 hoursASTM D570%0.5
Dissipation FactorASTM D1501MHz0.005
Test MethodUnitGuideline Value
HardnessASTM D2240Shore D86
Tensile Strength at yield 73°FASTM D638psi11400
Tensile ModulusASTM D638psi425000
Elongation at BreakASTM D638%5
Flexural StrengthASTM D790psi16000
Flexural ModulusASTM D790psi1050000
Compressive StrengthASTM D695psi15000
Rockwell HardnessASTM D78586
Rockwell HardnessASTM D785R120
Shear StrengthASTM D732psi8000
Izod Impact, NotchedASTM D256ft-lb/in1.0
Coefficient of Friction, Dynamic0.2
Test MethodUnitGuideline Value
Thermal Conductivityin/hr/ft2 /°F1.7
Coefficient of Linear Thermal ExpansionASTM D696in/in/°F x10-54,4
Melting Point°F330
Continuous Service Temperature, Air°F200
Deflection Temperature at 1.8Mpa (264psi)ASTM D648°F300
Flammability, UL941/8 inchHB
Test MethodUnitGuideline Value
Dielectric constantASTM D1501MHz3.7
Dielectric strengthASTM D149V/mil400
Surface resistivityASTM D257Ohm/cm104
Test MethodUnitGuideline Value
FDANo
NSFNo
USDANo

Contact

You have the option of attaching files to your message. The files have to be JPEG, PNG, BMP, PDF-documents. Please be sure that you only add files up to 8 MB

Information on data protection can be found here.


 
Search

Refine Results

Contact

Share

Print to PDF

Newsletter Registration

Select Website

Roechling_Industrial_Banner.jpg
Plastics for technical Applications

Industrial