Sustarin® C - ASTM

POM-C

QR-Code

Characteristics

  • Chemical resistance
  • Good dimensional stability
  • Low moisture absorption
  • Good sliding properties

Technical Specifications Sustarin® C - ASTM

Test MethodUnitGuideline Value
DensityASTM D792g / cm31.41
Water Absorption 24 hoursASTM D570%0.2
Dissipation FactorASTM D1501MHz0.004
Water Absorption SaturationASTM D570%0.9
Test MethodUnitGuideline Value
HardnessASTM D2240Shore D85
Tensile Strength at yield 73°FASTM D638psi9500
Tensile ModulusASTM D638psi400000
Elongation at BreakASTM D638%40
Flexural StrengthASTM D790psi12000
Flexural ModulusASTM D790psi400000
Compressive StrengthASTM D695psi15000
Rockwell HardnessASTM D78588
Rockwell HardnessASTM D785R120
Shear StrengthASTM D732psi8000
Izod Impact, NotchedASTM D256ft-lb/in1.2
Coefficient of Friction, Dynamic0.21
Test MethodUnitGuideline Value
Thermal Conductivityin/hr/ft2 /°F1.6
Coefficient of Linear Thermal ExpansionASTM D696in/in/°F x10-55.5
Melting Point°F330
Continuous Service Temperature, Air°F180
Deflection Temperature at 1.8Mpa (264psi)ASTM D648°F225
Deflection Temperature at 1.8Mpa (66psi)ASTM D648°F320
Flammability, UL941/8 inchHB
Test MethodUnitGuideline Value
Dielectric constantASTM D1501MHz3.8
Dielectric strengthASTM D149V/mil450
Surface resistivityASTM D257Ohm/cm1016
Test MethodUnitGuideline Value
FDAYes
NSFNo
USDAYes

Contact

You have the option of attaching files to your message. The files have to be JPEG, PNG, BMP, PDF-documents. Please be sure that you only add files up to 8 MB

Information on data protection can be found here.


 
Search

Refine Results

Contact

Share

Print to PDF

Newsletter Registration

Select Website

Roechling_Industrial_Banner.jpg
Plastics for technical Applications

Industrial