Test Method | Unit | Guideline Value | |
---|---|---|---|
Densité | DIN EN ISO 1183-1 | g / cm3 | 1,06 |
Flammability | UL 94 | HB | |
Moisture Absorption (23°C, 50% RH) | DIN EN ISO 62 | % | 0,06 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Yield stress | DIN EN ISO 527 | MPa | 30 |
Elongation at break | DIN EN ISO 527 | % | >50 |
Tensile modulus of elasticity | DIN EN ISO 527 | MPa | 1500 |
Notched impact strength | ISO 179-1/1eA | kJ / m2 | 17 |
Shore hardness | DIN EN ISO 868 | scale D | 78 |
Ball indentation hardness (H358/30) | DIN EN ISO 2039-1 | MPa | 70 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Coefficient of linear thermal expansion | DIN 53752 | 10-6 / K | 70 - 90 |
Vicat softening temperature | DIN EN ISO 306, Vicat B | °C | 115 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Dielectric constant | IEC 60250 | 2,7 | |
Volume resistivity | DIN EN 62631-3-1 | Ω * cm | 1015 |
Surface resistivity | DIN EN 62631-3-2 | Ω | >1015 |